Plastic Pipes Conference Association # 2021 Amsterdam
Shuhei Nishida, Shintaro Iwasaki, Hidefumi Yamanaka, Takahiro Kasatani
Polyethylene pipelines have been used for natural gas service applications for over 40 years in Japan. It is thought that they will continue to be used widely for many years. Therefore, it is important to confirm the conditions of the existing pipelines being used for the long term. In this study, polyethylene pipes comprising two types of resin and installed for a long term (more than 30 years) in Japan were investigated. Certain physical properties of these polyethylene pipes (such as the Charpy impact strength and melt mass flow rate (MFR)) changed in comparison with the properties of unused pipes of the same age. In contrast, the results regarding the full notch creep test (FNCT) of these pipes were approximately equal to those of the unused pipes. These results suggest that although the physical properties of polyethylene pipes buried for a long period of up to 30 years changed, the creep characteristics, which are more important for the life of the pipes, hardly changed. Therefore, these polyethylene pipes can be used for years to come.
Related papers
Author(s) : A. Marangoni
The quality of infrastructures is a key driver for maximizing the performance of the utilities networks and minimizing the environmental impacts associated with their operation. The water and sewer pipes are key network elements to guarantee a satisfactory service to the citizens. Their end-of-life management is an...
Author(s) : Li, Yanjun, Xiang, Aimin, Xu, HaiyunBeijing, Xie, Jianling, Ho, Kinman, Xu, HaiyunBeijing
It is necessary to evaluate the impact resistance of plastics pipes as they have the potential to be damaged by hitting or colliding during storage, transportation and installation. As a well-established test method, the Charpy impact strength of unnotched test pieces cut from thermoplastics pipes is determined...
Author(s) : A. Taraiya, P. Degenhart, M. Soliman, M. Boerakker, R. Handstanger, R. Kleppinger
Since the introduction of polyolefins for pressure pipes, continuous improvements have been made to meet ever-higher demands on their performance and to expand their application window beyond their original scope, mostly based on new resin formulations. Today, we also continue to push the limit to provide better...
Author(s) : Derek Muckle
A technical program has been undertaken to provide evidence on the suitability of polyethylene pipe and fitting systems for the distribution of hydrogen fuel gas. The underlying principle has been to evaluate material in the form of a pipe and to consider the performance of the pipe and of the welded jointing systems...
Author(s) : Peter Hubbard, Linqing Luo, Andrew Yeskoo, Kenichi Soga, Krista (Moita) Araica, Gus Cicala, Marshall McLeod
Seismically active faults pose a risk to buried water pipelines that can be complicated to quantify. Fault type, slip rate, pipeline geometry, and soil conditions all factor into a complex soil-pipeline interaction. For critical pipelines that cross faults, high-density polyethylene (HDPE) has become an attractive...
Author(s) : Anders Andtbacka, Peter Sejersen
In the late nineties a study of the behavior of buried thermoplastics pipes was carried out. The project had input and participants from both the plastic pipe industry as well as from external organizations. Six external leading experts in the field of pipeline design, not necessarily plastics pipes design, have been...
Author(s) : Dominique GUEUGNAUT, Pascal AUSSANT, Romuald BOUAFFRE, Myriam BECHROURI
Concerns regarding the environment and sustainable development have revived interest in the reprocessing and re-use of polymer materials from manufactured objects that have reached the end of their operating life. Within this framework, formal professional agreements have been put in place at global level under the...
Author(s) : Paul J. Freudenthaler, Joerg Fischer, Mathias Eder, Reinhold W. Lang
For controlled water disinfection, typically chlorine is used and preliminary studies demonstrate its aging and crack growth acceleration effects on polyolefin pipe materials [1, 2]. Although the use of recycled plastics is not prohibited in some ISO standards for polyolefin piping systems [3–5], only small amounts...
Author(s) : Mike Troughton, Amir Khamsehnezhad, Changyi Yu
When butt fusion welding polyethylene (PE) pipes in the field, it is often specified that the pipes must undergo fusibility testing in all combinations of suppliers, diameters and thicknesses before being fused in production. This is a very onerous and expensive task, but must be carried out to ensure that the PE...
Author(s) : James F. Mason, Akshay Ponda, Hermann van Laak, Buc Slay
The effects of liquid hydrocarbons on long term strength of pipe grade thermoplastic resins is an important consideration when designing pressure pipe for use in the oil and gas industry. There is an extensive body of work going back several decades descri bing these effects for pipe grade polyethylenes, and all...
Author(s) : Ernst van der Stok
For PE 100-RC, two tests are still under development for pipes: the point load test (PLT) and the accelerated notch pipe test (aNPT). The PLT was developed by a project group consisting of manufacturers and end users. The PLT determines the resistance to point loads as they can occur in practice. An earlier study...
Author(s) : S. Nestelberger, J. Cheng
The Point Load Test (PLT) [ 1, 2] was designed to simulate the SCG (slow crack growth) failure initiated by a rock pressing into the exterior wall of a polymer pipe. Today’s PE materials sustain long PLT testing times, due to its high SCG resistance design. Consequently, an accelerated “PLT+” with the support...
Author(s) : Dr. Holger Brüning, Serge Hascoët, Yann Delanne, Didier Nozahic, Jawdat Mansour, José Santana
RTE operates, maintains and develops the French electricity network, including the High and very High Voltage cable lines. Their network is the largest in Europe and includes over 6400 km of underground HV links operated in 2018. The company is modernizing and developing its network by investing 1.5 billion euros per...
Author(s) : Gerald Pinter, Johannes Wiener, Florian Arbeiter, Abhishek Tiwari, Otmar Kolednik
For pipe applications, catastrophic failure due to crack growth has to be prevented by all means. Techniques to develop new and even tougher pipe materials are explored in this contribution. The aim is to create a multi-layer architecture, that exhibits high toughness as well as damage tolerance towards sharp notches....
Author(s) : Stephan Kneck, Henrik Iskov
It has become ever clearer that the resources of natural gas are an energy source, which will be less important in the future due to limitations in use of natural reserves. In order to prepare for the future the gas industry is looking at the alternative fuel gases, one such fuel gas is hydrogen. In order to prepare...
Author(s) : Christian Schalich
Plastic pipes for infrastructure and building applications are precisely specified with regards to wall thickness and diameter. Pipe manufacturers use different measuring methods in order to ensure the required dimensional accuracy and maintain a constant high quality. This paper introduces a measuring system based on...
Author(s) : Mario Messiha, Britta Gerets, Jan Heimink, Andreas Frank, Florian Arbeiter, Gerald Pinter
A majority of field failure of viscoelastic plastic pipes can be attributed to slow crack growth (SCG) and has become crucial in terms of characterization of newly developed materials – particularly, if they are designed for pressurized pipe applications. In this study, investigations in terms of SCG resistances...
Author(s) : M. Eckes & Dr. B. Baudrit, Dr. M. Troughton & D. Wylie, H. van Laak & J. Fritz
Unplasticized polyamide 12 (PA-U12) is increasingly being used in pipe applications, especially in the gas sector. However, the material behavior in the usual quality tests for pipe welds has not yet been thoroughly investigated. For this reason, two research institutes, worked in cooperation with a manufacturer of...
Author(s) : Suleyman Deveci, Nisha Preschilla, Sulistiyanto Nugroho, Birkan Eryigit
Carbon black (CB) has been used as a perfect and the cheapest solution to prevent photo degradation of polyethylene against UV light exposure. The effect of carbon black on the mechanical properties of polyethylene pipes was studied extensively, but only on well dispersed and distributed carbon black...
Author(s) : Lukas Travnicek, Pavel Hutar, Jan Poduska, Andreas Frank, Florian Arbeiter, Jaroslav Kucera, Jiri Sadilek, Gerald Pinter, Lubos Nahlik
The application of recycled material in pressure piping systems has been considered lately – it was suggested, that the recycled polyethylene could be used as a part of a multilayer pipe together with virgin material. This type of pressure pipes is not availableon the market yet, so their properties can be only...